Q235钢(基材)/粉末环氧舟山全浸区8年去除表面附着物后未清洗腐蚀产物前腐蚀图谱
(
0
/0)
5秒
您已经浏览完所有图片
时间:2017-07-12 15:35:13 | 浏览次 | 已有
条评论
Q235钢(基材)/粉末环氧舟山全浸区8年去除表面附着物后未清洗腐蚀产物前腐蚀图谱
上一图集
下一图集
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/4dd6a7bf981e040e5c1c910a6bb33235.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/4dd6a7bf981e040e5c1c910a6bb33235.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/4dd6a7bf981e040e5c1c910a6bb33235.jpg
1
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/d2293032cbcb6e8fe0054c0e5da1a645.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/d2293032cbcb6e8fe0054c0e5da1a645.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/d2293032cbcb6e8fe0054c0e5da1a645.jpg
2
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/5de67e7da48962d5843dd64da6cd5e14.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/5de67e7da48962d5843dd64da6cd5e14.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/5de67e7da48962d5843dd64da6cd5e14.jpg
3
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/cba3450095b419804ddc2eb53a86b5ab.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/cba3450095b419804ddc2eb53a86b5ab.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/cba3450095b419804ddc2eb53a86b5ab.jpg
4
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/a8d712ecf335a7a5dbbb1d4c7e9854ff.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/a8d712ecf335a7a5dbbb1d4c7e9854ff.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/a8d712ecf335a7a5dbbb1d4c7e9854ff.jpg
5
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/356f281b3a3633ccef192245bf23cf46.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/356f281b3a3633ccef192245bf23cf46.jpg
http://data.ecorr.org/d/file/edata/05/maps/2017-07-12/356f281b3a3633ccef192245bf23cf46.jpg
6
腐蚀图谱
涂镀层试样西双版纳大气环境8年腐蚀图谱
2017-10-27
薄板试样西双版纳大气环境8年腐蚀图谱
2017-10-27
锻铝试样西双版纳大气环境8年腐蚀图谱
2017-10-27
各涂镀层试样西沙大气环境8年试验腐蚀图谱
2017-07-19
各涂镀层试样广州大气环境8年试验腐蚀图谱
2017-07-19
各涂镀层试样沈阳大气环境8年试验腐蚀图谱
2017-07-19
更多>>