首页
>
元数据
>
图谱数据
>
腐蚀图谱
成都土壤试验站投样二年未处理试样图谱
(
0
/0)
5秒
您已经浏览完所有图片
时间:2013-10-10 18:30:22 | 浏览次 | 已有
条评论
成都土壤试验站投样二年后未处理的试样
上一图集
下一图集
环氧粉末 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32102.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32102.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32102.jpg
1
环氧粉末 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32103.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32103.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32103.jpg
2
X80 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32111.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32111.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32111.jpg
3
X80 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32113.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32113.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32113.jpg
4
X70 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32115.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32115.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32115.jpg
5
X70 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32117.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32117.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32117.jpg
6
Q235B 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32118.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32118.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32118.jpg
7
Q235B 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32120.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32120.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32120.jpg
8
1Cr13 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32122.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32122.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32122.jpg
9
1Cr13 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32123.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32123.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32123.jpg
10
430 不锈钢 面1
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32128.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32128.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32128.jpg
11
430 不锈钢 面2
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32132.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32132.jpg
http://data.ecorr.org/uploads/allimg/2013/10/08/34-13100Q32132.jpg
12
腐蚀图谱
涂镀层试样西双版纳大气环境8年腐蚀图谱
2017-10-27
薄板试样西双版纳大气环境8年腐蚀图谱
2017-10-27
锻铝试样西双版纳大气环境8年腐蚀图谱
2017-10-27
各涂镀层试样西沙大气环境8年试验腐蚀图谱
2017-07-19
各涂镀层试样广州大气环境8年试验腐蚀图谱
2017-07-19
各涂镀层试样沈阳大气环境8年试验腐蚀图谱
2017-07-19
更多>>